Conveniently located in Clifton, NJ, off Routes 3, 21 and 17, right outside Manhattan, serving Brooklyn and QueensOff Routes 3, 21 and 17, right outside Manhattan40 Colorado Street, Clifton, NJ(973) 841-4442Visit40 Colorado Street, Clifton, NJConveniently located in Clifton, NJ, off Routes 3, 21 and 17, right outside Manhattan, serving Brooklyn and QueensOff Routes 3, 21 and 17, right outside ManhattanDrop-offMonday-Friday, 7am-7pmCall or text(973) 841-4442
Two of the crew strapping a bundle of red powder-coated pipes on the shop floor.

Services

Sandblasting and powder coating on steel, aluminum and iron, done in our own building in Clifton, New Jersey. Nothing is sent out.

Request a quote

The process, step by step

Most finish failures start between steps: steel that rusted after blasting, a part pulled before cure, a crate that chipped the edges. Here every step happens in one building, by one crew, in this order.

  1. Inspection and masking

    Checked in against your photo, drawing or notes.

    Parts are checked against your photo, drawing or notes on arrival. Threads, bearing surfaces and anything that has to stay bare are masked before they go near the blast room.

  2. Pre-treatment

    Parts are degreased and given a phosphate pre-treatment, using BCI products. Aluminum gets its own pre-treatment.

    Parts are degreased and given a phosphate pre-treatment in house, using pre-treatment products from BCI. Aluminum gets its own pre-treatment.

  3. Coating

    Sprayed electrostatically, so the powder wraps to edges and inside corners.

    Powder is applied electrostatically. The part is grounded and the charged powder wraps to it, which is how the inside corners and back faces get covered. How a part is racked decides whether that happens evenly.

  4. Curing

    Baked until the film is fully hardened and bonded to the metal.

    The part is held in the oven until the metal itself reaches the temperature the powder manufacturer specifies, and stays there long enough for the film to crosslink. This is the step that turns powder into a hard, bonded finish. A part pulled early looks finished, but the film never fully hardens: it chips at the edges and softens under solvent.

  5. Inspection and packing

    Wrapped, crated and labeled in the order you’ll install it.

    Film thickness is measured in mils and checked against your specification. The part is then wrapped, crated and labeled in the order you are installing it.

Have parts that need powder coating? Send us a photo.

Send a drawing. Get a price and a ready date.

Got a part to coat? Send a photo.

Send it over. We’ll price it.

You can also call us, text us, or stop by. Our team will quote your project and confirm lead times.

Rough sizes are fine.